Tensile Stress 40.07 MPa

@Strain 0.700 %,
Temperature 80.0 °C
5812 psi

@Strain 0.700 %,
Temperature 176 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 40.07 MPa

@Strain 0.900 %,
Temperature 90.0 °C
5812 psi

@Strain 0.900 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 40.07 MPa

@Strain 2.35 %,
Temperature 150 °C
5812 psi

@Strain 2.35 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I..