Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 40.83 MPa

@Strain 2.30 %,
Temperature 100 °C
5922 psi

@Strain 2.30 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 40.83 MPa

@Strain 0.550 %,
Temperature 90.0 °C
5922 psi

@Strain 0.550 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Tensile Stress 40.83 MPa

@Strain 0.550 %,
Temperature 90.0 °C
5922 psi

@Strain 0.550 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Tensile Stress 40.83 MPa

@Strain 1.40 %,
Temperature 150 °C
5922 psi

@Strain 1.40 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..