Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 65.1 MPa @Strain 0.670 %, Temperature 40.0 °C |
9440 psi @Strain 0.670 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Tensile Stress | 65.1 MPa @Strain 3.12 %, Temperature 90.0 °C |
9440 psi @Strain 3.12 %, Temperature 194 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |