Polymer Property : Tensile Stress = 6521 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 44.96 MPa

@Strain 3.41 %,
Temperature 90.0 °C
6521 psi

@Strain 3.41 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..
Tensile Stress 44.96 MPa

@Strain 20.95 %,
Temperature 40.0 °C
6521 psi

@Strain 20.95 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..
Tensile Stress 44.96 MPa

@Strain 2.20 %,
Temperature 150 °C
6521 psi

@Strain 2.20 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers