Mechanical Properties Metric English Comments
Tensile Stress 46.25 MPa

@Strain 3.57 %,
Temperature 40.0 °C
6708 psi

@Strain 3.57 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 46.25 MPa

@Strain 2.23 %,
Temperature 150 °C
6708 psi

@Strain 2.23 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Tensile Stress 46.25 MPa

@Strain 2.23 %,
Temperature 150 °C
6708 psi

@Strain 2.23 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..