Polymer Property : Tensile Stress = 6790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 46.8 MPa

@Strain 1.48 %,
Temperature 90.0 °C
6790 psi

@Strain 1.48 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Tensile Stress 46.8 MPa

@Strain 6.32 %,
Temperature 150 °C
6790 psi

@Strain 6.32 %,
Temperature 302 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 46.8 MPa

@Strain 0.880 %,
Temperature 23.0 °C
6790 psi

@Strain 0.880 %,
Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers