Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 75.8 MPa @Strain 4.27 %, Temperature 150 °C |
11000 psi @Strain 4.27 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Tensile Stress | 75.8 MPa @Strain 0.0500 % |
11000 psi @Strain 0.0500 % |
Process Temperature T4 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |
|||
Tensile Stress | 75.8 MPa @Strain 0.0500 % |
11000 psi @Strain 0.0500 % |
Process Temperature T1 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |