Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.62 MPa @Strain 300 % |
1250 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® A9875H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 8.62 MPa @Strain 0.320 %, Temperature 23.0 °C |
1250 psi @Strain 0.320 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Tensile Stress | 8.62 MPa @Strain 204.54 %, Temperature 100 °C |
1250 psi @Strain 204.54 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.62 MPa @Strain 2.15 %, Temperature 150 °C |
1250 psi @Strain 2.15 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.62 MPa @Strain 44.89 %, Temperature 120 °C |
1250 psi @Strain 44.89 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.62 MPa @Strain 1.25 %, Temperature 150 °C |
1250 psi @Strain 1.25 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 8.62 MPa @Strain 100 % |
1250 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 8.62 MPa @Strain 100 % |
1250 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P45D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |