Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | >= 8.96 MPa @Strain 100 % |
>= 1300 psi @Strain 100 % |
ASTM D412 Method A |
Seals Eastern 7265 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito.. |
|||
Tensile Stress | 8.96 MPa @Strain 0.110 %, Temperature 23.0 °C |
1300 psi @Strain 0.110 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |