Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 80.67 MPa @Strain 0.630 %, Temperature 0.000 °C |
11700 psi @Strain 0.630 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |