Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 80.4 MPa @Strain 1.03 %, Temperature 40.0 °C |
11700 psi @Strain 1.03 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 81.0 MPa @Strain 10.0 %, Temperature 100 °C |
11700 psi @Strain 10.0 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 81.0 MPa @Strain 4.00 % |
11700 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Tensile Stress | 80.68 MPa @Strain 3.12 %, Temperature -40.0 °C |
11700 psi @Strain 3.12 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Tensile Stress | 80.4 MPa @Strain 3.70 %, Temperature -40.0 °C |
11700 psi @Strain 3.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Tensile Stress | 81.0 MPa @Strain 19.2 %, Temperature -40.0 °C |
11700 psi @Strain 19.2 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 80.68 MPa @Strain 3.12 %, Temperature -40.0 °C |
11700 psi @Strain 3.12 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Tensile Stress | 81.0 MPa @Strain 0.740 %, Temperature 0.000 °C |
11700 psi @Strain 0.740 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 80.8 MPa @Strain 0.822 %, Temperature 23.0 °C |
11700 psi @Strain 0.822 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6
(Unverified Data**) 35% Glass Reinforced Polyamide 66 Developed for Electrical and Electronics ApplicationsZytel 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics application.. |
|||
Tensile Stress | 80.8 MPa @Strain 0.822 %, Temperature 23.0 °C |
11700 psi @Strain 0.822 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Tensile Stress | 80.8 MPa @Strain 3.20 %, Temperature 23.0 °C |
11700 psi @Strain 3.20 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Stress | 80.7 MPa @Strain 0.700 %, Temperature 23.0 °C |
11700 psi @Strain 0.700 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Stress | 80.8 MPa @Strain 3.40 %, Temperature 150 °C |
11700 psi @Strain 3.40 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Stress | 81.0 MPa @Strain 17.0 %, Temperature -20.0 °C |
11700 psi @Strain 17.0 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 80.8 MPa @Strain 1.80 %, Temperature 23.0 °C |
11700 psi @Strain 1.80 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 80.67 MPa @Strain 0.630 %, Temperature 0.000 °C |
11700 psi @Strain 0.630 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |