Polymer Property : Tensile Stress = 84.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 84.5 MPa

@Strain 18.2 %,
Temperature -20.0 °C
12300 psi

@Strain 18.2 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 84.5 MPa

@Strain 5.60 %,
Temperature -20.0 °C
12300 psi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Tensile Stress 84.5 MPa

@Strain 5.60 %,
Temperature -20.0 °C
12300 psi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Tensile Stress 84.5 MPa

@Strain 3.50 %,
Temperature 23.0 °C
12300 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..