Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 86.0 MPa @Strain 50.0 %, Temperature -40.0 °C |
12500 psi @Strain 50.0 %, Temperature -40.0 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |