Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 86.3 MPa @Strain 1.40 %, Temperature -20.0 °C |
12500 psi @Strain 1.40 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Tensile Stress | 86.5 MPa @Strain 1.60 %, Temperature 0.000 °C |
12500 psi @Strain 1.60 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 86.2 MPa @Strain 0.00100 % |
12500 psi @Strain 0.00100 % |
|
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta.. |
|||
Tensile Stress | 86.0 MPa @Strain 50.0 %, Temperature -40.0 °C |
12500 psi @Strain 50.0 %, Temperature -40.0 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Tensile Stress | 86.4 MPa @Strain 2.79 %, Temperature 23.0 °C |
12500 psi @Strain 2.79 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |