Polymer Property : Tensile Stress = 8850 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 61.0 MPa

@Strain 6.93 %,
Temperature -20.0 °C
8850 psi

@Strain 6.93 %,
Temperature -4.00 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 61.0 MPa

@Strain 8.00 %,
Temperature 120 °C
8850 psi

@Strain 8.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
Tensile Stress 61.0 MPa

@Strain 0.960 %,
Temperature 23.0 °C
8850 psi

@Strain 0.960 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
Tensile Stress 61.0 MPa

@Strain 1.38 %,
Temperature 60.0 °C
8850 psi

@Strain 1.38 %,
Temperature 140 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 61.0 MPa

@Strain 1.04 %,
Temperature 40.0 °C
8850 psi

@Strain 1.04 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 61.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
8850 psi

@Strain 50.0 %,
Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..