Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 90.3 MPa @Strain 1.87 %, Temperature 0.000 °C |
13100 psi @Strain 1.87 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 90.3 MPa @Strain 0.100 %, Temperature 1204 °C |
13100 psi @Strain 0.100 %, Temperature 2199 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |