Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 62.07 MPa @Strain 3.90 %, Temperature 150 °C |
9003 psi @Strain 3.90 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 62.07 MPa @Strain 16.38 %, Temperature 0.000 °C |
9003 psi @Strain 16.38 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |