Mechanical Properties Metric English Comments
Tensile Stress 65.07 MPa

@Strain 1.42 %,
Temperature 90.0 °C
9438 psi

@Strain 1.42 %,
Temperature 194 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided ..
Tensile Stress 65.07 MPa

@Strain 1.82 %,
Temperature 90.0 °C
9438 psi

@Strain 1.82 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..