Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
15 sec; ASTM D2240
53
53
ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
510 mm/min; ASTM D638
Tensile Strength 14.5 MPa

@Strain 100 %
2100 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 330 %
330 %
510 mm/min; ASTM D638
Tear Strength 114 kN/m
650 pli
Die C, 510 mm/min; ASTM D624
Compression Set 60 %

@Temperature 23.0 °C,
Time 79200 sec
60 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.758 GPa
110 ksi
ASTM D1043
0.310 GPa

@Temperature -13.0 °C
45.0 ksi

@Temperature 8.60 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 188 °C
351 - 370 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features General Purpose
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose
Users viewing this material also viewed the following: