Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.2804 MPa | 40.67 psi | ASTM D790 |
Sekisui PIOCELAN OP-30DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |