Sekisui PIOCELAN OP-30DB Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN OP-30DB Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Automotive partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.4218 MPa
61.18 psi
ASTM D3575
Elongation at Break 7.8 %
7.8 %
ASTM D3575
Flexural Strength 0.2804 MPa
40.67 psi
ASTM D790
Flexural Modulus 0.012589 GPa
1.8259 ksi
ASTM D790
Compressive Strength 0.1746 MPa

@Strain 25.0 %
25.33 psi

@Strain 25.0 %
ASTM D3575
0.2381 MPa

@Strain 50.0 %
34.54 psi

@Strain 50.0 %
ASTM D3575
0.4844 MPa

@Strain 75.0 %
70.26 psi

@Strain 75.0 %
ASTM D3575
Compression Set 40.5 %
40.5 %
ASTM D3575
Descriptive Properties Value Comments
Color Black
Range of center value of pre-expanded particles 0.15-0.2 in