Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | initial |
Malvern Minerals Nylon with Novacite® L-337 Quartz Filler Product data demonstrates the effect of the Novacite® (untreated lamellar quartz) filler. A separate entry demonstrates the effect of treated Novakup® filler in nylon. The specific nylon use.. |
|||
Flexural Strength | 68.9 - 82.7 MPa | 10000 - 12000 psi | ASTM D790 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | |
SGL Carbon Group EI 2100 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES HiFill® HDPE GF15 50100 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES HiFill® HDPE GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D 790 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Flexural Strength | 69.0 MPa | 10000 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr.. |
|||
Flexural Strength | 68.9 MPa | 10000 psi | ASTM D-790 |
Axiall UV-6670 Rigid PVC, Molding Georgia Gulf UV-6670 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ashley Polymers Ashlene® ABS 243 Medium impact, high flow, rigid. Suitable for injection molding of appliances, automotive components, office machines, switch boxes and panels.Data provided by the manufacturer |
|||
Flexural Strength | 68.9 MPa | 10000 psi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Flexural Strength | 68.9 - 82.7 MPa | 10000 - 12000 psi | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Flexural Strength | 68.9 - 159 MPa | 10000 - 23000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Resinoid 2010 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |