Mechanical Properties Metric English Comments
Flexural Strength 55.0 - 75.0 MPa
7980 - 10900 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Flexural Strength 55.0 - 75.0 MPa
7980 - 10900 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Flexural Strength 55.0 - 75.0 MPa
7980 - 10900 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Flexural Strength 55.0 - 75.0 MPa
7980 - 10900 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Flexural Strength 65.0 - 75.0 MPa
9430 - 10900 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
Flexural Strength 55.0 - 75.0 MPa

@Temperature 1000 °C
7980 - 10900 psi

@Temperature 1830 °F
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics
For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend..
Flexural Strength 73.0 - 75.0 MPa
10600 - 10900 psi
ASTM D790M
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure
Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo..