Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 55.0 - 75.0 MPa | 7980 - 10900 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 55.0 - 75.0 MPa | 7980 - 10900 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 55.0 - 75.0 MPa | 7980 - 10900 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 55.0 - 75.0 MPa | 7980 - 10900 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 65.0 - 75.0 MPa | 9430 - 10900 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Flexural Strength | 55.0 - 75.0 MPa @Temperature 1000 °C |
7980 - 10900 psi @Temperature 1830 °F |
|
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend.. |
|||
Flexural Strength | 73.0 - 75.0 MPa | 10600 - 10900 psi | ASTM D790M |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |