Polymer Property : Flexural Strength = 11250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 77.57 MPa
11250 psi
ASTM D790
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 77.57 MPa
11250 psi
ASTM D790
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Flexural Strength 77.57 MPa
11250 psi
ASTM D790
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..