Flexural Strength 118.9 MPa
17250 psi
ASTM D790
Nilit Polynil® P200 High Viscosity Nylon 66
Description: High viscosityApplication: Semi-finished and FilmInformation provided by NILIT.
Flexural Strength 118.9 MPa
17250 psi
ASTM D790
Nilit Polynil® P230 High Viscosity Nylon 66
Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various..
Flexural Strength 118.9 MPa
17250 psi
ASTM D790
Nilit Polynil® P240 High Viscosity Nylon 66
Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri..