Material Notes:
Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various food approvals.Key characteristics: Viscosity number 280 cm3/grLow gel contentVarious food contact approvalsHigh heat stabilityInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Viscosity Measurement 230
230
relative viscosity (formic acid); ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
Elongation at Break 142 %
142 %
ASTM D638
Tensile Modulus 2.71 GPa
393 ksi
ASTM D638
Flexural Strength 118.9 MPa
17250 psi
ASTM D790
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Izod Impact, Notched (ISO) 6.93 kJ/m²
3.30 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648