Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.0 - 87.0 MPa | 12300 - 12600 psi | ASTM D790M |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3 Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Flexural Strength | 83.8 - 86.7 MPa | 12200 - 12600 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Flexural Strength | 83.8 - 86.7 MPa | 12200 - 12600 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |