Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 84.0 MPa | <= 12200 psi | ISO 178 |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid) Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne |
|||
Flexural Strength | 84.0 MPa | 12200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | <= 84.0 MPa | <= 12200 psi | ISO 178 |
Polykemi AB POLYabs HD2 ABS Information provided by Polykemi AB |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **)&l Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Kotec Carbotex K-30F5 Polycarbonate, Wear Resistant Features: Wear resistance, TranslucentApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation provided by Kotec Corporation |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1000 PC (Asia Pacific) |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Styron Pulse® 2000 ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific) PA6 based unfilled GTX for Wheel cover |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
Polyplastics Duranex® 601SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 83.8 - 86.7 MPa | 12200 - 12600 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Ashley Polymers Ashlene® 735LD Nylon 6 An impact modified, plasticized copolymer with improved impact resistance for injection molding.Data provided by the manufacturer |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ASTM D790 |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D790 |
Chase Plastics CP Pryme® N213GL (COND, 50% RH) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 84.1 MPa | 12200 psi | ASTM D-790 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |
|||
Flexural Strength | 84.0 MPa | 12200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |