Flexural Strength 13.0 MPa
1890 psi
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Flexural Strength 13.0 MPa
1890 psi
ASTM D790
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding
Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp..
Flexural Strength >= 13.0 MPa
>= 1890 psi
MarkeTech Repton 314 Mullite
Brand 314 features: Superior hot creep.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the..
Flexural Strength 13.0 MPa
1890 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer
LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant.
Flexural Strength 13.0 MPa
1890 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Strength 13.0 MPa
1890 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Flexural Strength 13.0 MPa
1890 psi
Shandong Guangyin PA 1212 Nylon Resin
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab..
Flexural Strength 13.0 MPa
1890 psi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Flexural Strength 13.0 MPa
1890 psi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Flexural Strength 13.0 MPa
1890 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP)
LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s).
Flexural Strength 13.0 MPa
1890 psi
Olsen; ASTM D747
UBE J1019 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength 13.0 MPa
1890 psi
Olsen; ASTM D747
UBE J2522 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..