Flexural Strength 115.1 MPa
16690 psi
Method 1, 0.05"/min; ASTM D790
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer
Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren..