Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 189.33 MPa | 27460 psi | ASTM D790 |
E-Polymers SEPAZ® K365GM 60% Glass Fiber/Calcium Carbonate Reinforced General Purpose PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |