Polymer Property : Flexural Strength = 2.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 2.50 MPa
363 psi
@ 25 kg/m<sup>2</sup>; ASTM DC201
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Flexural Strength 2.50 MPa
363 psi
@ 25 kg/m<sup>2</sup>; ASTM DC201
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Flexural Strength 2.50 MPa
363 psi
SAE J949
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 2.50 MPa
363 psi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 2.50 MPa
363 psi
SAE J949
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..