Mechanical Properties Metric English Comments
Flexural Strength 188 MPa
27300 psi
102 mm Span, 3 mm/min; ASTM D790
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement  (discontinued **)
ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th..
Flexural Strength 188 MPa
27300 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 188 MPa
27300 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 188 MPa
27300 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 188 MPa
27300 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.
Flexural Strength 188 MPa
27300 psi
ISO 178
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Flexural Strength 188 MPa
27300 psi
ISO 178
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Flexural Strength 188 MPa
27300 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC
LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated.
Flexural Strength 188 MPa
27300 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC
LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved