Flexural Strength 29.1 MPa
4220 psi
ASTM D790
Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet)
Flexural Strength 29.1 MPa
4220 psi
ASTM D790
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 29.1 MPa
4220 psi
ASTM D790
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 29.1 MPa
4220 psi
ASTM D790
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne