PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.549 - 0.748 g/cc
0.549 - 0.748 g/cc
Cellular; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength, Yield 14.9 MPa
2160 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.14 GPa
165 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 29.1 MPa
4220 psi
ASTM D790
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Izod Impact, Notched 0.210 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.393 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy 6.67 J/cm

@Temperature 23.0 °C
0.0125 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C

@Thickness 3.18 mm
149 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Forms Cellular, Free Blow
Powder
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following: