Mechanical Properties Metric English Comments
Flexural Strength 293 MPa
42500 psi
ASTM D790
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Strength 293 MPa
42500 psi
ASTM D790
Kolon KOPA® KN333C22 CF Reinforced Nylon 66
Carbon 22%, high strengthApplications Cylinder piston partsInformation provided by API-Kolon.
Flexural Strength 293 MPa
42500 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber.
Flexural Strength 293 MPa
42500 psi
2 mm/min; ISO 178
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber
SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties..
Flexural Strength 293 MPa
42500 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific)
LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber.