Material Notes:
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.Applications: Components for automotive and aircraft enginesTransmissionFarming, off-road and construction equipmentIndustrial machineryElectric motors, pumps and compressorsBusiness machines such as laser pointers and high speed copy machinesElectronic and semiconductor transport mediaAnalytical and medical equipmentConveyors and textile equipmentInformation provided by Mitsui.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.070 %
0.070 %
24 hours, 23°C, 60% RH
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 203 MPa
29400 psi
ASTM D638
Tensile Strength, Ultimate 137.3 MPa

@Temperature 150 °C
19910 psi

@Temperature 302 °F
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
3.0 %

@Temperature 150 °C
3.0 %

@Temperature 302 °F
ASTM D638
Flexural Strength 293 MPa
42500 psi
ASTM D790
201 MPa

@Temperature 150 °C
29200 psi

@Temperature 302 °F
ASTM D790
Flexural Modulus 10.4 GPa
1510 ksi
ASTM D790
9.32 GPa

@Temperature 150 °C
1350 ksi

@Temperature 302 °F
ASTM D790
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 23.0 °C
9.44 µin/in-°F

@Temperature 73.4 °F
MD; ASTM D696
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Melting Point 388 °C
730 °F
Maximum Service Temperature, Air >= 260 °C
>= 500 °F
Heat distortion temperature, load unknown; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 390 - 420 °C
734 - 788 °F
Injection molding, extrusion