Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 202 MPa | 29300 psi | ISO 178 |
Celanese Celcon® GC25T POM, 25% Glass Reinforced
(Unverified Data**) Celcon® GC25T is a 25% glass fiber coupled acetal copolymer grade. It offers higher strength than the standard Celcon GC25-A. Celcon GC25T is FDA approved. Celcon GC25T is also exceptionally resis.. |
|||
Flexural Strength | 202 MPa | 29300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 HS L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Flexural Strength | 202 MPa | 29300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 202 MPa | 29300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Flexural Strength | 202 MPa | 29300 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 202 MPa | 29300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 202 MPa | 29300 psi | ISO 178 |
Polyplastics Duranex® 7400F Polybutylene Terephthalate (PBT), Low friction, Low wear, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 202 MPa | 29300 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 441 Glass Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.32% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 202 MPa | 29300 psi | ASTM D790 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Strength | 202 MPa | 29300 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 202 MPa | 29300 psi | ISO 178 |
Celanese Celcon® GC25T POM, 25% Glass Reinforced Celcon« GC25T is a 25% glass fiber coupled acetal copolymer grade. It offers higher strength than the standard Celcon GC25-A. Celcon GC25T is FDA approved. Celcon GC25T is also exceptionally resis.. |