Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.32% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 123 MPa
17800 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
Flexural Strength 202 MPa
29300 psi
ASTM D790
Flexural Modulus 11.2 GPa
1620 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 - 268 °C
496 - 514 °F
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
Copyright © lookpolymers.com All Rights Reserved