Polymer Property : Flexural Strength = 31.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 31.6 MPa
4580 psi
ISO 178
ExxonMobil Exxtralâ„¢ BMU 141 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s..