Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2150 MPa | 312000 psi | |
China Tungsten YG546 Tungsten Carbide Good toughness, high strength, capable of resisting high impact load, Roughing of stainless steel and cast irons.Information provided by China Tungsten |