Mechanical Properties Metric English Comments
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Strength 20.0 - 34.0 MPa

@Strain 5.00 %
2900 - 4930 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..