Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Multibase Nylex™ 2185 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Network Polymers Nylon 6040 Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
I. Stern SH432HG High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingHigh glossApplicationsThermoformed containers and lids for food packagingCustom extruded sheetABS replace.. |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Chase Plastics CP Pryme® N100L (COND, 50% RH) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Total PSI 945E Polystyrene Polystyrene 945E is a high impact polystyrene designed for applications requiring extra toughness without sacrificing mechanical properties. Excellent falling dart impact combined with the high glos.. |
|||
Flexural Strength | 43.4 MPa | 6300 psi | ASTM D790 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |