Material Notes:
Description: Natural NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Water Absorption 1.3 %
1.3 %
24 hours Immersion; ASTM D570
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.9 MPa
5200 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Strength 43.4 MPa
6300 psi
ASTM D790
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
1/8 in specimen; ASTM D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 43.3 °C
110 °F
0.125 in bar; ASTM D648