Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 313 MPa
45400 psi
ASTM D790
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Strength 313 MPa
45400 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.