Mechanical Properties Metric English Comments
Flexural Strength 5.17 MPa
750 psi
ASTM D790
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Strength 5.17 MPa
750 psi
Diaphragm Burst Strength
Saint-Gobain COHRlastic® CF3320 Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
Flexural Strength 5.17 MPa
750 psi
Diaphragm Burst Strength
Saint-Gobain COHRlastic® CF4032 General Purpose Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
Flexural Strength 5.17 MPa
750 psi
Diaphragm Burst Strength
Saint-Gobain COHRlastic® CF4451 High Surface Resistivity Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
Flexural Strength 5.17 MPa
750 psi
Diaphragm Burst Strength
Saint-Gobain COHRlastic® CF4050 General Purpose Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
Flexural Strength 5.17 MPa
750 psi
Diaphragm Burst Strength
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..