Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 5.17 MPa | 750 psi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Strength | 5.17 MPa | 750 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF3320 Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Flexural Strength | 5.17 MPa | 750 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF4032 General Purpose Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Flexural Strength | 5.17 MPa | 750 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF4451 High Surface Resistivity Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Flexural Strength | 5.17 MPa | 750 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF4050 General Purpose Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Flexural Strength | 5.17 MPa | 750 psi | Diaphragm Burst Strength |
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |