Flexural Strength 0.350 MPa
50.8 psi
48 hour silo aging time
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
Flexural Strength 0.350 MPa
50.8 psi
64 hours silo aging time
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..