Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 524 MPa | 76000 psi | Transverse Rupture |
Pacific Sintered Materials F-240-S Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-25All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 524 MPa | 76000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 524 MPa | 76000 psi | 0° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |